一种 γ'/γ'' 相强化镍基高温合金的蠕变行为
周生玉, 胡明昊, 李冲, 丁海民, 郭乾应, 刘永长

Creep Behavior of a Ni-Based Superalloy with Strengthening of γ' and γ'' Phases
ZHOU Shengyu, HU Minghao, LI Chong, DING Haimin, GUO Qianying, LIU Yongchang
图3 不同热处理态镍基高温合金试样的高温蠕变曲线
Fig.3 High-temperature creep curves (750 oC, 120 MPa) of Ni-based superalloy specimens after different heat treatments
(a) creep time-strain curves (b) creep time-strain rate curves