微重力条件下Gd-Co-Ti合金原位粒子复合凝固组织的形成
孙昊, 江鸿翔, 赵九洲, 张丽丽, 何杰

Formation of In Situ Particle Composite Solidification Microstructure of Gd-Co-Ti Alloy Under Microgravity Conditions
SUN Hao, JIANG Hongxiang, ZHAO Jiuzhou, ZHANG Lili, HE Jie
图6 Gd-Co-Ti体系溶质Co和Ti质量比wCowTi = 1∶1的垂直截面图和平衡条件下Gd-2%Co-2%Ti合金的凝固过程示意图
Fig.6 Verical section of wCowTi = 1∶1 for the phase diagram of the Gd-Co-Ti system (a) and schematic of the solidification process of the Gd-2%Co-2%Ti alloy under equilibrium conditions (b) (wCo and wTi—mass fractions of solutes Co and Ti, respectively. L1 + L2 represents liquid-liquid phase transformation region. T—temperature. T1, T2, T3, and T4 represent the equilibrium binodal line temperature, onset temperature of liquid-liquid-solid phase transformation, and temperatures of the invariant reactions 1 and 2, respectively)