微重力条件下Gd-Co-Ti合金原位粒子复合凝固组织的形成 |
| 孙昊, 江鸿翔, 赵九洲, 张丽丽, 何杰 |
|
Formation of In Situ Particle Composite Solidification Microstructure of Gd-Co-Ti Alloy Under Microgravity Conditions |
| SUN Hao, JIANG Hongxiang, ZHAO Jiuzhou, ZHANG Lili, HE Jie |
| 图5 Gd-2%Co-2%Ti合金样品中富TiCo相粒子的数密度(ND)随样品尺寸(D)的变化 |
| Fig.5 Number density (ND) of the TiCo-rich particles in the Gd-2%Co-2%Ti alloy sample vs sample size (D) |
|