On the Homogeneous Nucleation Characteristics of Al Droplets During Isothermal Crystallization
WANG Shucheng, PENG Ping
图7 不同形状临界晶核的内部结构和界面形态示意图
Fig.7 Snapshots of internal structures (a1-c1) of critical nuclei and their interfacial morphologies (a2-c2) (Green, red, and gray balls represent fcc, hcp, and other atoms, respectively. The digits on the ball are the identification codes of atoms)
(a1, a2) chainlike (b1, b2) lamellar (c1, c2) ellipsoidal/half-spherical