Al液滴等温结晶的形核特征分析
王书成, 彭平

On the Homogeneous Nucleation Characteristics of Al Droplets During Isothermal Crystallization
WANG Shucheng, PENG Ping
图3 等温结晶过程中Al液滴和Al液体的双体分布函数(g(r))和晶体原子占比
Fig.3 Pair distribution function (g(r)) curves (a, c) and percentages of fcc, hcp, bcc, and ico atoms (b, d) during the isothermal crystallization of Al droplet (a, b) and Al bulk (c, d) (r—distance from the central atom. fcc, hcp, bcc, and ico represent faced-centered cubic, hexagonal close-packed, body-centered cubic, and icosahedral, respectively)