连铸结晶器内Ar气泡破碎-聚合和捕获行为的数值模拟
徐涛, 邓安元, 李阳, 王恩刚

Numerical Simulation of Ar Bubbles Fragmentation-Polymerization and Trapping Behavior in Continuous Casting Mold
XU Tao, DENG Anyuan, LI Yang, WANG Engang
图21 不同水口浸入深度下结晶器内被气泡捕获数量和不同直径气泡的捕获占比
Fig.21 Trapped bubble volumes (a) and capture ratios of bubbles with different diameters (b) in the mold with different nozzle immersion depths