连铸结晶器内Ar气泡破碎-聚合和捕获行为的数值模拟
徐涛, 邓安元, 李阳, 王恩刚

Numerical Simulation of Ar Bubbles Fragmentation-Polymerization and Trapping Behavior in Continuous Casting Mold
XU Tao, DENG Anyuan, LI Yang, WANG Engang
图7 结晶器内的Ar气泡分布和含气率分布
Fig.7 Distribution of Ar bubbles (a) and gas volume fraction (b) of the mold (The casting speed is 1.4 m/min, the Ar blowing rate is 10 L/min, the nozzle angle is -15°, and the nozzle immersion depth is 180 mm. Vf—volume fraction)