连铸结晶器内Ar气泡破碎-聚合和捕获行为的数值模拟
徐涛, 邓安元, 李阳, 王恩刚

Numerical Simulation of Ar Bubbles Fragmentation-Polymerization and Trapping Behavior in Continuous Casting Mold
XU Tao, DENG Anyuan, LI Yang, WANG Engang
图5 气泡碰撞-弹开实验[25]和模拟结果
Fig.5 Bubble collision-bounce experiment results[25] (a) and simulation results (b) (Red circles represent the process of bubble collision-bounce)