基于深冷轧制备的高强韧高氮奥氏体不锈钢的力学行为 |
| 赵今涛, 孙利芳, 何竹风, 刘玉杰, 马小柏, 申勇峰, 贾楠 |
|
Mechanical Behavior of Cryogenic Rolling Processed High Nitrogen Austenitic Stainless Steel with High Strength and Good Toughness |
| ZHAO Jintao, SUN Lifang, HE Zhufeng, LIU Yujie, MA Xiaobai, SHEN Yongfeng, JIA Nan |
| 图7 HOMO、A850和CRR10%材料断口形貌的SEM像 |
| Fig.7 SEM images showing the fracture morphologies of the HOMO (a), A850 (b), and CRR10% (c) materials |
|