基于深冷轧制备的高强韧高氮奥氏体不锈钢的力学行为
赵今涛, 孙利芳, 何竹风, 刘玉杰, 马小柏, 申勇峰, 贾楠

Mechanical Behavior of Cryogenic Rolling Processed High Nitrogen Austenitic Stainless Steel with High Strength and Good Toughness
ZHAO Jintao, SUN Lifang, HE Zhufeng, LIU Yujie, MA Xiaobai, SHEN Yongfeng, JIA Nan
图6 HOMO、A850和CRR10%材料拉伸变形前后的XRD谱
Fig.6 XRD spectra of the HOMO, A850, and CRR10% materials before (a) and after (b) tensile testing