基于深冷轧制备的高强韧高氮奥氏体不锈钢的力学行为 |
| 赵今涛, 孙利芳, 何竹风, 刘玉杰, 马小柏, 申勇峰, 贾楠 |
|
Mechanical Behavior of Cryogenic Rolling Processed High Nitrogen Austenitic Stainless Steel with High Strength and Good Toughness |
| ZHAO Jintao, SUN Lifang, HE Zhufeng, LIU Yujie, MA Xiaobai, SHEN Yongfeng, JIA Nan |
| 图2 A750、A850、A950、HOMO和CRR10%材料的工程应力-应变曲线、真应力-应变曲线及加工硬化率曲线 |
| Fig.2 Egineering stress-strain curves (a), true stress-strain curves (b), work hardening rate vs true strain curves (c) of the A750, A850, A950, HOMO, and CRR10% materials at various states |
|