基于深冷轧制备的高强韧高氮奥氏体不锈钢的力学行为 |
| 赵今涛, 孙利芳, 何竹风, 刘玉杰, 马小柏, 申勇峰, 贾楠 |
|
Mechanical Behavior of Cryogenic Rolling Processed High Nitrogen Austenitic Stainless Steel with High Strength and Good Toughness |
| ZHAO Jintao, SUN Lifang, HE Zhufeng, LIU Yujie, MA Xiaobai, SHEN Yongfeng, JIA Nan |
| 图1 高氮奥氏体不锈钢热轧板的加工路线示意图 |
| Fig.1 Schematic of processing routes for the high nitrogen austenitic stainless steel (HNASS) hot-rolled plate (CR—cold rolling, CRR—cryogenic rolling) |
|