形变球化对珠光体钢在模拟货油舱内底板环境中腐蚀行为和力学性能的影响
郭佳明, 陈楠, 何小燕, 魏洁, 陈慧琴, 董俊华, 柯伟

Effect of Deformation Spheroidization Treatment on the Corrosion Behavior and Mechanical Properties of Pearlite Steel in Simulated Cargo Oil Tank Inner Substrate Environment
GUO Jiaming, CHEN Nan, HE Xiaoyan, WEI Jie, CHEN Huiqin, DONG Junhua, KE Wei
表2 T8钢和T1#钢的大、小角度晶界比例及平均晶粒尺寸
Table 2 Proportions of LAGB and HAGB (fLAGB and fHAGB) and average grain sizes (d) of T8 steel and T1# steel
SteelfLAGBfHAGBd
%%μm
T812.387.734.18
T1#5.994.12.74