形变球化对珠光体钢在模拟货油舱内底板环境中腐蚀行为和力学性能的影响
郭佳明, 陈楠, 何小燕, 魏洁, 陈慧琴, 董俊华, 柯伟

Effect of Deformation Spheroidization Treatment on the Corrosion Behavior and Mechanical Properties of Pearlite Steel in Simulated Cargo Oil Tank Inner Substrate Environment
GUO Jiaming, CHEN Nan, HE Xiaoyan, WEI Jie, CHEN Huiqin, DONG Junhua, KE Wei
图13 T8钢和T1#钢在模拟溶液中的年腐蚀速率随浸泡时间的变化
Fig.13 Annual corrosion rate (v) as a function of immersion time (t) of T8 steel and T1# steel in simulated solution