形变球化对珠光体钢在模拟货油舱内底板环境中腐蚀行为和力学性能的影响 |
| 郭佳明, 陈楠, 何小燕, 魏洁, 陈慧琴, 董俊华, 柯伟 |
|
Effect of Deformation Spheroidization Treatment on the Corrosion Behavior and Mechanical Properties of Pearlite Steel in Simulated Cargo Oil Tank Inner Substrate Environment |
| GUO Jiaming, CHEN Nan, HE Xiaoyan, WEI Jie, CHEN Huiqin, DONG Junhua, KE Wei |
| 图10 T8钢浸泡120和216 h后除锈前后表面腐蚀形貌的SEM像 |
| Fig.10 SEM surface corrosion images of T8 steel after immersion for 120 h (a1, a2) and 216 h (b1, b2) before (a1, b1) and after (a2, b2) rust removal |
|