增材制造难变形高温合金GH4975的裂纹形成及其愈合机制 |
| 叶献文, 姚志浩, 王洪瑛, 王子成, 张砻耀, 董建新 |
|
Crack Formation and Healing Mechanisms in Additively Manufactured Hard-Deformed Ni-Based Superalloy GH4975 |
| YE Xianwen, YAO Zhihao, WANG Hongying, WANG Zicheng, ZHANG Longyao, DONG Jianxin |
| 图9 热等静压态和打印态TiC-GH4975试样经不同温度热压缩后显微组织的SEM像 |
| Fig.9 SEM images of TiC-GH4975 HIPed (a, c) and as-build (b, d) samples after hot compression at 1160 oC (a, b) and 1200 oC (c, d) |
|