增材制造难变形高温合金GH4975的裂纹形成及其愈合机制
叶献文, 姚志浩, 王洪瑛, 王子成, 张砻耀, 董建新

Crack Formation and Healing Mechanisms in Additively Manufactured Hard-Deformed Ni-Based Superalloy GH4975
YE Xianwen, YAO Zhihao, WANG Hongying, WANG Zicheng, ZHANG Longyao, DONG Jianxin
图4 GH4975和TiC-GH4975打印态试样晶粒形貌的EBSD像
Fig.4 EBSD images of as-build GH4975 (a) and TiC-GH4975 (b) samples