表2 AB、DA和SA试样中奥氏体晶面间距 (nm)
Table 2 Intergranular spacings of austenite in AB, DA, and SA states
IntergranularABDASA
spacing
(111)0.207970.207880.20765
(200)0.180240.180020.17994
(220)0.127290.127280.12711
(311)0.108560.108540.10840
(222)0.103880.103690.10375