选区激光熔化GH4169高温合金的微观组织和力学性能 |
| 孙勇飞, 向超, 张涛, 吴文伟, 邹志航, 刘金鹏, 孙桂芳, 蒲吉斌, 韩恩厚 |
|
Microstructures and Mechanical Properties of GH4169 Superalloy Manufactured by Selective Laser Melting |
| SUN Yongfei, XIANG Chao, ZHANG Tao, WU Wenwei, ZOU Zhihang, LIU Jinpeng, SUN Guifang, PU Jibin, HAN En-Hou |
| 图9 GH4169高温合金AB、DA和SA试样的高温工程应力-应变曲线 |
| Fig.9 High-temperature engineering stress-strain curves of GH4169 superalloy specimens in AB, DA, and AS states |
|