选区激光熔化GH4169高温合金的微观组织和力学性能 |
| 孙勇飞, 向超, 张涛, 吴文伟, 邹志航, 刘金鹏, 孙桂芳, 蒲吉斌, 韩恩厚 |
|
Microstructures and Mechanical Properties of GH4169 Superalloy Manufactured by Selective Laser Melting |
| SUN Yongfei, XIANG Chao, ZHANG Tao, WU Wenwei, ZOU Zhihang, LIU Jinpeng, SUN Guifang, PU Jibin, HAN En-Hou |
| 图3 GH4169高温合金打印态(AB)、直接时效(DA)和固溶+时效(SA)试样的XRD谱 |
| Fig.3 XRD spectra of GH4169 superalloy specimens in AB, DA, and SA states (Inset is a partially magnified spectra) |
|