堆垛层错能对CrMnFeCoNi系高熵合金动态力学性能与变形机制的影响 |
| 尹仕攀, 孟泽宇, 贺竞瑶, 李泽洲, 张帆, 程兴旺 |
|
Effect of Stacking Fault Energy on the Dynamic Mechanical Properties and Deformation Mechanisms of CrMnFeCoNi High-Entropy Alloys |
| YIN Shipan, MENG Zeyu, HE Jingyao, LI Zezhou, ZHANG Fan, CHENG Xingwang |
| 图10 5 × 103 s-1应变率加载条件下,真应变为0.25时,CrMnFeCoNi和Cr26Mn20Fe20Co20Ni14高熵合金的TEM分析 |