堆垛层错能对CrMnFeCoNi系高熵合金动态力学性能与变形机制的影响
尹仕攀, 孟泽宇, 贺竞瑶, 李泽洲, 张帆, 程兴旺

Effect of Stacking Fault Energy on the Dynamic Mechanical Properties and Deformation Mechanisms of CrMnFeCoNi High-Entropy Alloys
YIN Shipan, MENG Zeyu, HE Jingyao, LI Zezhou, ZHANG Fan, CHENG Xingwang
图9 5 × 103 s-1应变率加载条件下,真应变为0.25时,CrMnFeCoNi和Cr26Mn20Fe20Co20Ni14高熵合金变形组织的EBSD分析
Fig.9 EBSD analyses of the deformed microstructure under dynamic compression with a strain rate of 5 × 103 s-1 and true strain of 0.25 of CrMnFeCoNi (a, c) and Cr26Mn20Fe20Co20Ni14 (b, d) HEAs
(a, b) IQ maps (c, d) KAM maps