LPSO相含量对挤压态Mg-Y-Zn-Mn合金耐腐蚀性能的影响 |
| 江舒佳, 杨宏冉, 李传强, 王乃光, 王德升 |
|
Effect of Long-Period Stacking Ordered Phase Content on the Corrosion Resistance of As-Extruded Mg-Y-Zn-Mn Alloy |
| JIANG Shujia, YANG Hongran, LI Chuanqiang, WANG Naiguang, WANG Desheng |
| 图12 挤压态WZ21M、WZ42M和WZ84M合金在3.5%NaCl 溶液中浸泡24 h并去除腐蚀产物的截面SEM像 |
| Fig.12 Low (a-c) and locally high (d-f) magnified cross-sectional SEM images of as-extruded WZ21M (a, d), WZ42M (b, e), and WZ84M (c, f) alloys after immersion in 3.5%NaCl solution for 24 h and subsequently removing products |
|