LPSO相含量对挤压态Mg-Y-Zn-Mn合金耐腐蚀性能的影响 |
| 江舒佳, 杨宏冉, 李传强, 王乃光, 王德升 |
|
Effect of Long-Period Stacking Ordered Phase Content on the Corrosion Resistance of As-Extruded Mg-Y-Zn-Mn Alloy |
| JIANG Shujia, YANG Hongran, LI Chuanqiang, WANG Naiguang, WANG Desheng |
| 图8 挤压态WZ21M、WZ42M和WZ84M合金在3.5%NaCl溶液中浸泡不同时间后的OM原位观察像 |
| Fig.8 In situ OM images of the corrosion morphologies of as-extruded WZ21M (a1-a5), WZ42M (b1-b5), and WZ84M (c1-c5) alloys immersed in 3.5%NaCl solution for 1 h (a1-c1), 2 h (a2-c2), 4 h (a3-c3), 8 h (a4-c4), and 24 h (a5-c5) |
|