LPSO相含量对挤压态Mg-Y-Zn-Mn合金耐腐蚀性能的影响
江舒佳, 杨宏冉, 李传强, 王乃光, 王德升

Effect of Long-Period Stacking Ordered Phase Content on the Corrosion Resistance of As-Extruded Mg-Y-Zn-Mn Alloy
JIANG Shujia, YANG Hongran, LI Chuanqiang, WANG Naiguang, WANG Desheng
图2 挤压态Mg-2Y-1Zn-0.1Mn (WZ21M)、Mg-4Y-2Zn-0.1Mn (WZ42M)和Mg-8Y-4Zn-0.1Mn (WZ84M)合金的XRD谱
Fig.2 XRD spectra of as-extruded Mg-2Y-1Zn-0.1Mn (WZ21M), Mg-4Y-2Zn-0.1Mn (WZ42M), and Mg-8Y-4Zn-0.1Mn (WZ84M) alloys (LPSO—long-period stacking ordered)