O含量对Ti2448合金时效析出行为及力学性能的影响
李丹, 宫得伦, 郝玉琳

Effect of O Content on the Aging Precipitation Behavior and Mechanical Properties of Ti2448 Alloy
LI Dan, GONG Delun, HAO Yulin
图10 873 K、10 min + 773 K、1 h双步热处理后Ti2448-HO合金中析出相的TEM像和SAED花样
Fig.10 Bright field (a) and dark field (b) TEM images of precipitates in Ti2448-HO alloys after annealing at 873 K for 10 min and followed by aging at 773 K for 1 h (Inset in Fig.10b shows the corresponding SAED pattern taken along [01¯1] β zone axis)