(AlCrTaTiZr)N x 阻氚涂层制备及其表面氢同位素吸附
张建东, 席晓翀, 凌永生, 曾繁荣, 单卿, 贾文宝

Preparation of (AlZrTaTiZr)N x Tritium Barrier Coating and Adsorption of Hydrogen Isotope on the Surface
ZHANG Jiandong, XI Xiaochong, LING Yongsheng, ZENG Fanrong, SHAN Qing, JIA Wenbao
图9 不同H2覆盖度下稳定吸附后涂层的体积模量(B)、Young's模量(E)、剪切模量(G)、Poisson比(ν)和B / G
Fig.9 Bulk modulus (B)(a), Young's modulus (E)(b), shear modulus (G)(c), and Poisson's ratio (ν) and B / G (d) of the coating after stable adsorption under different H2 coverages