(AlCrTaTiZr)N x 阻氚涂层制备及其表面氢同位素吸附 |
| 张建东, 席晓翀, 凌永生, 曾繁荣, 单卿, 贾文宝 |
|
Preparation of (AlZrTaTiZr)N x Tritium Barrier Coating and Adsorption of Hydrogen Isotope on the Surface |
| ZHANG Jiandong, XI Xiaochong, LING Yongsheng, ZENG Fanrong, SHAN Qing, JIA Wenbao |
| 图4 H2在(AlCrTaTiZr)N表面的吸附位点示意图 |
| Fig.4 Schematic of adsorption sites of H2 on the surface of (AlCrTaTiZr)N |
|