Ti表面Ag/g-C3N4 共敏化TiO2 纳米膜的构筑及其光电化学行为
官自超, 胡娟, 时海燕, 董士刚, 刘亚安, 王霞, 金飘, 杜荣归

Fabrication and Photoelectrochemical Properties of Ag/g-C3N4 Co-Sensitized TiO2 Nanotube Composite Film on Ti Substrate
GUAN Zichao, HU Juan, SHI Haiyan, DONG Shigang, Liu Ya'an, WANG Xia, JIN Piao, DU Ronggui
表1 不同膜样品表面成分分析结果 (atomic fraction / %)
Table 1 Chemical compositions of the prepared films
SampleTiOCNAg
TiO248.4351.57---
g-C3N4/TiO222.8729.9433.8113.38-
Ag/TiO245.6353.81--0.56
Ag/g-C3N4/TiO223.4330.7633.5812.000.23