Ti表面Ag/g-C3N4 共敏化TiO2 纳米膜的构筑及其光电化学行为 |
| 官自超, 胡娟, 时海燕, 董士刚, 刘亚安, 王霞, 金飘, 杜荣归 |
|
Fabrication and Photoelectrochemical Properties of Ag/g-C3N4 Co-Sensitized TiO2 Nanotube Composite Film on Ti Substrate |
| GUAN Zichao, HU Juan, SHI Haiyan, DONG Shigang, Liu Ya'an, WANG Xia, JIN Piao, DU Ronggui |
| 图10 403SS在0.5 mol/L NaCl溶液中的等效电路模型 |
| Fig.10 Equivalent circuit models for 403SS in the 0.5 mol/L NaCl solution (Rs—solution resistance, Rct—charge transfer resistance, R—film resistance, CPE and CPE1—constant phase elements) (a) uncoupled (b) coupled to the illuminated film |
|