Ti表面Ag/g-C3N4 共敏化TiO2 纳米膜的构筑及其光电化学行为 |
| 官自超, 胡娟, 时海燕, 董士刚, 刘亚安, 王霞, 金飘, 杜荣归 |
|
Fabrication and Photoelectrochemical Properties of Ag/g-C3N4 Co-Sensitized TiO2 Nanotube Composite Film on Ti Substrate |
| GUAN Zichao, HU Juan, SHI Haiyan, DONG Shigang, Liu Ya'an, WANG Xia, JIN Piao, DU Ronggui |
| 图7 TiO2膜、g-C3N4/TiO2复合膜、Ag/TiO2复合膜和Ag/g-C3N4/TiO2复合膜在间歇白光照射下的光电流响应 |
| Fig.7 Transient photocurrent responses of the TiO2, g-C3N4/TiO2, Ag/TiO2, and Ag/g-C3N4/TiO2 films under intermittent white light illumination (i—current density, t—time) |
|