选区激光熔化Ni58Cr23Fe10W5Ti2Ta1Nb1 多主元合金的裂纹形成机理及抑制
林美, 郭博静, 王志军, 李俊杰, 王雷, 王锦程, 何峰

Crack Mechanism and Control Strategy for Ni58Cr23Fe10W5-Ti2Ta1Nb1 Multi-Principal Element Alloy by Selective Laser Melting
LIN Mei, GUO Bojing, WANG Zhijun, LI Junjie, WANG Lei, WANG Jincheng, HE Feng
表1 复合合金粉末及选区激光熔化成形块体的理论成分和实际成分 (mass fraction / %)
Table 1 Designed composition and chemical composition of alloy powder and SLMed sample
SampleCrFeWTiTaNbBCONi

Designed composition of powder

Practical composition of powder

18.7408.75211.5302.1312.8361.4560.360--Bal.
18.6008.89011.4002.0403.5001.6100.3100.0010.140Bal.
Practical composition of SLMed block19.0008.96010.5002.1603.3401.5900.2100.0590.078Bal.