选区激光熔化Ni58Cr23Fe10W5Ti2Ta1Nb1 多主元合金的裂纹形成机理及抑制 |
| 林美, 郭博静, 王志军, 李俊杰, 王雷, 王锦程, 何峰 |
|
Crack Mechanism and Control Strategy for Ni58Cr23Fe10W5-Ti2Ta1Nb1 Multi-Principal Element Alloy by Selective Laser Melting |
| LIN Mei, GUO Bojing, WANG Zhijun, LI Junjie, WANG Lei, WANG Jincheng, HE Feng |
| 图14 在P = 280 W、v = 1000 mm/s、t = 0.04 mm、h = 0.07 mm成形工艺下TiB2改性Ni58Cr23Fe10W5Ti2-Ta1Nb1合金的熔池形貌 |
| Fig.14 Melt pool morphology of SLMed Ni58Cr23Fe10-W5Ti2Ta1Nb1 alloy adding 1%TiB2 nanoparticles at the process parameters of P = 280 W, v = 1000 mm/s, t = 0.04 mm, h = 0.07 mm |
|