选区激光熔化Ni58Cr23Fe10W5Ti2Ta1Nb1 多主元合金的裂纹形成机理及抑制 |
| 林美, 郭博静, 王志军, 李俊杰, 王雷, 王锦程, 何峰 |
|
Crack Mechanism and Control Strategy for Ni58Cr23Fe10W5-Ti2Ta1Nb1 Multi-Principal Element Alloy by Selective Laser Melting |
| LIN Mei, GUO Bojing, WANG Zhijun, LI Junjie, WANG Lei, WANG Jincheng, HE Feng |
| 图11 选区激光熔化成形Ni58Cr23Fe10W5Ti2Ta1Nb1合金在Ev = 182.3 J/mm3下的应力分布特征 |
| Fig.11 Stress distribution characteristics of SLMed Ni58Cr23Fe10W5Ti2Ta1Nb1 alloy under Ev = 182.3 J/mm3 (a) kernel average misorientation (KAM) map (b) inverse pole figure (IPF) (Recrystallized grains are indicated by circles) |
|