选区激光熔化Ni58Cr23Fe10W5Ti2Ta1Nb1 多主元合金的裂纹形成机理及抑制 |
| 林美, 郭博静, 王志军, 李俊杰, 王雷, 王锦程, 何峰 |
|
Crack Mechanism and Control Strategy for Ni58Cr23Fe10W5-Ti2Ta1Nb1 Multi-Principal Element Alloy by Selective Laser Melting |
| LIN Mei, GUO Bojing, WANG Zhijun, LI Junjie, WANG Lei, WANG Jincheng, HE Feng |
| 图6 选区激光熔化成形Ni58Cr23Fe10W5Ti2Ta1Nb1合金在体能量密度Ev = 182.3 J/mm3 (激光功率P = 350 W、扫描速率v = 600 mm/s)下的裂纹分布特征 |
| Fig.6 Crack distribution characteristics of SLMed Ni58Cr23Fe10W5Ti2Ta1Nb1 alloy under volume energy density Ev = 182.3 J/mm3 (P = 350 W, v = 600 mm/s) (a) grain boundary distribution (The red lines and blue lines denote the high-angle grain boundaries (misorientation angle > 15°) and low-angle grain boundaries (misorientation angle 2°-15°), respectively) (b) misorientation between grain pairs that are present in Fig.6a |
|