选区激光熔化Ni58Cr23Fe10W5Ti2Ta1Nb1 多主元合金的裂纹形成机理及抑制 |
| 林美, 郭博静, 王志军, 李俊杰, 王雷, 王锦程, 何峰 |
|
Crack Mechanism and Control Strategy for Ni58Cr23Fe10W5-Ti2Ta1Nb1 Multi-Principal Element Alloy by Selective Laser Melting |
| LIN Mei, GUO Bojing, WANG Zhijun, LI Junjie, WANG Lei, WANG Jincheng, HE Feng |
| 图4 不同工艺参数下选区激光熔化成形Ni58Cr23Fe10W5Ti2Ta1Nb1合金缺陷的OM像 |
| Fig.4 OM images of SLMed Ni58Cr23Fe10W5Ti2Ta1Nb1 alloy under laser powers (P) of 210 W (a1-d1), 245 W (a2-d2), 280 W (a3-d3), 315 W (a4-d4), and 350 W (a5-d5) and scanning velocities (v) of 1200 mm/s (a1-a5), 1000 mm/s (b1-b5), 800 mm/s (c1-c5), and 600 mm/s (d1-d5) |
|