选区激光熔化Ni58Cr23Fe10W5Ti2Ta1Nb1 多主元合金的裂纹形成机理及抑制 |
| 林美, 郭博静, 王志军, 李俊杰, 王雷, 王锦程, 何峰 |
|
Crack Mechanism and Control Strategy for Ni58Cr23Fe10W5-Ti2Ta1Nb1 Multi-Principal Element Alloy by Selective Laser Melting |
| LIN Mei, GUO Bojing, WANG Zhijun, LI Junjie, WANG Lei, WANG Jincheng, HE Feng |
| 图2 TiB2纳米颗粒及1%TiB2纳米颗粒和Ni58Cr23Fe10W5Ti2Ta1Nb1合金粉末机械混合后的粉末形貌及EDS元素面扫描图 |
| Fig.2 Powder morphologies of TiB2 nanoparticles (a) and mechanical mixing of 1%TiB2 nanoparticle and Ni58Cr23Fe10- W5Ti2Ta1Nb1 alloy powder (b), and locally enlarged image of Fig.2b and corresponding EDS elemental mapping results (b1) |
|