Zr-0.75Sn-0.35Fe-0.15Cr-xNb合金在高温空气/蒸汽混合气氛中的氧化行为
俞强, 徐诗彤, 张佳楠, 姚美意, 胡丽娟, 谢耀平, 周邦新

Oxidation Behaviors of Zr-0.75Sn-0.35Fe-0.15Cr- xNb Alloys in High-Temperature Steam with Air
YU Qiang, XU Shitong, ZHANG Jianan, YAO Meiyi, HU Lijuan, XIE Yaoping, ZHOU Bangxin
表4 1000和1200 ℃下0Nb、0.15Nb、0.50Nb和1.0Nb合金在空气/蒸汽混合气氛和N2/蒸汽混合气氛[21]中的氧化增重与纯水蒸气气氛[19]中的氧化增重比值
Table 4 Ratios of oxidation mass gain of 0Nb, 0.15Nb, 0.50Nb, and 1.0Nb alloys in air/steam mixed atmosphere and N2/steam mixed atmosphere[21] to that in steam[19] at 1000 and 1200 oC
AlloyΔw(N2/steam)[21] / Δw(steam)[19]Δw(Air/steam) / Δw(steam)[19]
1000 oC, 3600 s1200 oC, 1800 s1000 oC, 3600 s1200 oC, 1800 s
0Nb10.23.915.13.5
0.15Nb15.33.322.33.3
0.50Nb8.43.124.13.1
1.0Nb15.93.932.13.8