Zr-0.75Sn-0.35Fe-0.15Cr-xNb合金在高温空气/蒸汽混合气氛中的氧化行为
俞强, 徐诗彤, 张佳楠, 姚美意, 胡丽娟, 谢耀平, 周邦新

Oxidation Behaviors of Zr-0.75Sn-0.35Fe-0.15Cr- xNb Alloys in High-Temperature Steam with Air
YU Qiang, XU Shitong, ZHANG Jianan, YAO Meiyi, HU Lijuan, XIE Yaoping, ZHOU Bangxin
表3 与0Nb合金相比,0.15Nb、0.30Nb、0.50Nb和1.0Nb合金在800~1200 ℃空气/蒸汽混合气氛中氧化的氧化增重变化百分数 (%)
Table 3 Compared to 0Nb alloy, the percentages of mass gain change for 0.15Nb, 0.30Nb, 0.50Nb, and 1.0Nb alloys oxidized in air/steam mixed atmosphere at 800-1200 oC
T / oCOxide time / sF0.15NbF0.30NbF0.50NbF1.0Nb
80018003.310.622.730.6
1080039.893.8265.1303.6
10001800-2.741.391.4-1.2
360024.969.791.768.6
1200180027.744.918.012.7