Zr-0.75Sn-0.35Fe-0.15Cr-xNb合金在高温空气/蒸汽混合气氛中的氧化行为
|
|
俞强, 徐诗彤, 张佳楠, 姚美意, 胡丽娟, 谢耀平, 周邦新
|
Oxidation Behaviors of Zr-0.75Sn-0.35Fe-0.15Cr- xNb Alloys in High-Temperature Steam with Air
|
|
YU Qiang, XU Shitong, ZHANG Jianan, YAO Meiyi, HU Lijuan, XIE Yaoping, ZHOU Bangxin
|
|
表2 Zr-0.75Sn-0.35Fe-0.15Cr-xNb合金在800~1200 ℃的空气/蒸汽混合气氛中的氧化动力学参数拟合结果
|
Table 2 Fitting results of oxidation kinetic parameters for Zr-0.75Sn-0.35Fe-0.15Cr-xNb alloys in air/steam mixed atmosphere at 800-1200 oC
|
|
| T / oC | Alloy | Transition | Transition point / s | lnKn | n |
|---|
| 800 | 0Nb | - | - | 3.31 | 0.62 | | 0.15Nb | - | - | 3.29 | 0.66 | | 0.30Nb | - | - | 3.17 | 0.74 | | 0.50Nb | - | - | 2.73 | 0.94 | | 1.0Nb | - | - | 2.77 | 0.95 | | 1000 | 0Nb | - | - | 4.50 | 1.11 | | 0.15Nb | Before transition | - | 4.02 | 1.00 | | | First transition | 666 | 1.76 | 1.92 | | | Second transition | 1968 | 4.95 | 1.03 | | 0.30Nb | Before transition | - | 4.42 | 1.11 | | | First transition | 594 | 3.51 | 1.54 | | | Second transition | 1320 | 4.88 | 1.12 | | 0.50Nb | Before transition | - | 4.53 | 1.17 | | | First transition | 696 | 3.03 | 1.79 | | | Second transition | 1572 | 6.53 | 0.72 | | 1.0Nb | Before transition | - | 4.20 | 1.09 | | | First transition | 1254 | 1.82 | 1.91 | | | Second transition | 2184 | 3.58 | 1.44 | | 1200 | 0Nb | Before transition | - | 5.83 | 0.97 | | | After transition | 354 | 6.13 | 0.80 | | 0.15Nb | Before transition | - | 6.09 | 0.98 | | | After transition | 354 | 6.46 | 0.77 | | 0.30Nb | Before transition | - | 6.52 | 0.96 | | | After transition | 312 | 7.09 | 0.64 | | 0.50Nb | Before transition | - | 6.08 | 0.98 | | | After transition | 312 | 6.53 | 0.72 | | 1.0Nb | Before transition | - | 6.00 | 0.98 | | | After transition | 282 | 6.29 | 0.80 |
|
|
|