Zr-0.75Sn-0.35Fe-0.15Cr-xNb合金在高温空气/蒸汽混合气氛中的氧化行为
俞强, 徐诗彤, 张佳楠, 姚美意, 胡丽娟, 谢耀平, 周邦新

Oxidation Behaviors of Zr-0.75Sn-0.35Fe-0.15Cr- xNb Alloys in High-Temperature Steam with Air
YU Qiang, XU Shitong, ZHANG Jianan, YAO Meiyi, HU Lijuan, XIE Yaoping, ZHOU Bangxin
图2 5种合金在800~1200 ℃的空气/蒸汽混合气氛中氧化后横截面显微组织的OM像
Fig.2 Cross-sectional OM images of 0Nb (a1-a3), 0.15Nb (b1-b3), 0.30Nb (c1-c3), 0.50Nb (d1-d3), and 1.0Nb (e1-e3) alloys after oxidation in air/steam mixed atmosphere
(a1-e1) 800 oC, 10800 s (a2-e2) 1000 oC, 3600 s (a3-e3) 1200 oC, 1800 s