室温和深冷轧制对纯Al再结晶{111}/{111}近奇异晶界的影响
李振想, 王卫国, Rohrer Gregory S, 洪丽华, 陈松, 林燕, 周邦新

Effects of Ambient and Cryogenic Rolling on {111}/{111} Near Singular Boundary Formation During Subsequent Recrystallization Annealing in Pure Aluminum
LI Zhenxiang, WANG Weiguo, Rohrer Gregory S, HONG Lihua, CHEN Song, LIN Yan, ZHOU Bangxin
图5 A和A1样品的轧面(A-ND和A1-ND)、横切面(A-RD和A1-RD)及纯Al粉末样品(Powder)的XRD谱
Fig.5 XRD spectra of sample A (a) and sample A1 (b) obtained from the rolling planes (A-ND and A1-ND), the planes perpendicular to rolling direction (A-RD and A1-RD), and from the sample of powdered pure aluminum (Powder) (ND—normal direction, RD—rolling direction)