Cr和Sc元素对钨基合金晶粒组织高温稳定性的影响
杜文力, 侯超, 李昱嵘, 韩铁龙, 宋晓艳

Effect of Cr and Sc on High-Temperature Stability of Grain Structure in W-Based Alloys
DU Wenli, HOU Chao, LI Yurong, HAN Tielong, SONG Xiaoyan
表1 不同温度下纯W、W-10Cr和W-5Cr-5Sc合金的晶粒长大指数(n)和晶粒长大激活能(Q)
Table 1 Grain growth indexes (n) and activation energies for grain growth(Q) of pure W, W-10Cr, and W-5Cr-5Sc alloys at different temperatures (T)
Sample

T

oC

n

Q

kJ·mol-1

W10007.91248.9
11002.3363.6
12002.5395.2
13002.7426.8
W-10Cr12005.9640.4
13003.5379.9
14004.0434.2
W-5Cr-5Sc12005.4555.5
13003.7376.8
14006.0611.1