Cr和Sc元素对钨基合金晶粒组织高温稳定性的影响
杜文力, 侯超, 李昱嵘, 韩铁龙, 宋晓艳

Effect of Cr and Sc on High-Temperature Stability of Grain Structure in W-Based Alloys
DU Wenli, HOU Chao, LI Yurong, HAN Tielong, SONG Xiaoyan
图10 W-5Cr-5Sc烧结态合金中三叉晶界处的微观组织TEM像及EDS分析
Fig.10 TEM image of the triple junction grain boundaries of W-5Cr-5Sc sintered alloy (a), EDS element maps of W (b), Cr (c), and Sc (d), and EDS line scan along arrow in Fig.10a (e)