Cr和Sc元素对钨基合金晶粒组织高温稳定性的影响 |
| 杜文力, 侯超, 李昱嵘, 韩铁龙, 宋晓艳 |
|
Effect of Cr and Sc on High-Temperature Stability of Grain Structure in W-Based Alloys |
| DU Wenli, HOU Chao, LI Yurong, HAN Tielong, SONG Xiaoyan |
| 图9 烧结态W-5Cr-5Sc合金微观组织的TEM像及EDS元素面分布图 |
| Fig.9 TEM image (a) and corresponding EDS elemental distribution maps of W (b), Cr (c), and Sc (d) of W-5Cr-5Sc sintered alloy (Circles in Fig.9a represent nanoparticles located at the triple grain boundaries) |
|