Cr和Sc元素对钨基合金晶粒组织高温稳定性的影响
杜文力, 侯超, 李昱嵘, 韩铁龙, 宋晓艳

Effect of Cr and Sc on High-Temperature Stability of Grain Structure in W-Based Alloys
DU Wenli, HOU Chao, LI Yurong, HAN Tielong, SONG Xiaoyan
图7 烧结态W-10Cr合金微观组织的TEM像及EDS元素面分布图
Fig.7 TEM image (a) and corresponding EDS elemental distribution maps of W (b) and Cr (c) of W-10Cr sintered alloy