Cr和Sc元素对钨基合金晶粒组织高温稳定性的影响 |
| 杜文力, 侯超, 李昱嵘, 韩铁龙, 宋晓艳 |
|
Effect of Cr and Sc on High-Temperature Stability of Grain Structure in W-Based Alloys |
| DU Wenli, HOU Chao, LI Yurong, HAN Tielong, SONG Xiaoyan |
| 图4 烧结态以及不同热处理温度保温2 h后纯W、W-10Cr和W-5Cr-5Sc合金的晶粒尺寸 |
| Fig.4 Grain sizes of pure W, W-10Cr, and W-5Cr-5Sc alloys after sintering and heat treatment at different temperatures for 2 h |
|