Cr和Sc元素对钨基合金晶粒组织高温稳定性的影响 |
| 杜文力, 侯超, 李昱嵘, 韩铁龙, 宋晓艳 |
|
Effect of Cr and Sc on High-Temperature Stability of Grain Structure in W-Based Alloys |
| DU Wenli, HOU Chao, LI Yurong, HAN Tielong, SONG Xiaoyan |
| 图2 烧结态纯W、W-10Cr和W-5Cr-5Sc合金的SEM像及晶粒尺寸分布 |
| Fig.2 SEM images (a, c, e) and distributions of grain size (b, d, f) of pure W (a, b), W-10Cr (c, d), and W-5Cr-5Sc (e, f) sintered alloys |
|