高 γ′相含量GH4151变形高温合金铸态组织与开裂敏感性分析
钟佳, 王法, 江河, 姚志浩, 董建新

Analyses of As-Cast Microstructure and Cracking Sensitivity of GH4151 Wrought Superalloy with High γ′ Phase Content
ZHONG Jia, WANG Fa, JIANG He, YAO Zhihao, DONG Jianxin
表2 铸态GH4151合金枝晶间各析出相的化学成分 (mass fraction / %)
Table 2 Chemical compositions of interdendritic precipitates in as-cast GH4151 alloy
PhaseCAlTiVCrCoNiNbMoW
Laves–1.21.60.421.122.225.312.213.72.3
η–6.58.1–3.612.661.06.51.20.5
γ/γ′ eutectic–9.77.3–3.012.763.13.11.00.1
MC56.30.110.80.30.30.41.628.90.80.5