高 γ′相含量GH4151变形高温合金铸态组织与开裂敏感性分析 |
| 钟佳, 王法, 江河, 姚志浩, 董建新 |
|
Analyses of As-Cast Microstructure and Cracking Sensitivity of GH4151 Wrought Superalloy with High γ′ Phase Content |
| ZHONG Jia, WANG Fa, JIANG He, YAO Zhihao, DONG Jianxin |
| 图9 直径410 mm的GH4151合金自耗锭在1120 ℃等温热压缩实验后的宏观形貌及不同相界面的SEM像(1 s-1应变速率、30%变形量) |
| Fig.9 Macro-morphology of cracked surface (a) and SEM images of different phase interfaces (b-e) of GH4151 alloy consumable ingot with a diameter of 410 mm after isothermal hot compression test at 1120 oC with strain rate of 1 s-1 and deformation of 30% (DRX—dynamic recrystallization) (b) MC/γ phase interface (c) Laves phase interface (d) γ/γ′ eutectic phase interface (e) η phase interface |
|